Chemical Resistant Conveyor Belt
Application
Suitable for conveying corrosive materials in chemical factories,cement plant,fertilizer plants,paper mills,mining industry,etc.

Technical Data
Physical property of cover rubber under hot air accelerated aging test(test condition:50℃*96h).
Class | Solution | Concentration | Covered Condition | The Change Rate Before And After Covered | |
Volume Expansivity | Strength Change Rate | ||||
A1 | (HCI) | 18% | 50℃x96h | ≥10% | ≤10% |
A2 | (H2SO4) | 50% | 50℃x96h | ≥10% | ≤10% |
A3 | (NaOH) | 48% | 50℃x96h | >10% | <10% |
ITEM | Breaking Strength(Mpa) | Elongation At Break(%) | Abrasion(mm3) | Hardness(Shore) |
Performance before aging | ≥14.0 | ≥400 | ≤250 | 60±5 |
Performance after aging | ≥12.0 | ≥350 | - | 60±5 |
Note: When the thickness of the cover rubber is 0.8mm-1.6mm,the sample thickness can be the maximum cut length,the tensile strength and elongation at break are allowed to be 15% lower than those in the table. |